論文- 庄子 哲雄 -
表示方法: 表示形式: 表示順:
件数:553件
[1986]
501.ボイラ過熱器管SUS316H鋼管の経年劣化.[日本機械学会論文集(A編),52(473),(1986),165-169]斎藤喜久,庄子哲雄,高橋秀明
502.流動海水環境における高張力鋼の腐食疲労.[防食技術,35,(1986),503-508]張 舜植, 庄子哲雄, 高橋秀明, 渡辺 豊
503.Cr-Mo-V鋼の遷移温度域における粒界割れ破壊靭性の試験片寸法効果.[鉄と鋼,72(11),(1986),1744-1750]下村慶一,庄子哲雄,高橋秀明,斎藤潔
504.極低温用構造材料溶接部の微視破壊過程と破壊靭性評価.[日本機械学会論文集(A編),52(473),(1986),170-173]大西慶太,庄子哲雄,高橋秀明
[1985]
505.Quantitative Prediction of Environmentally Assisted Cracking Base on Crack Tip Strain Rate.[PPCEAC,(1985),17-22]T. Shoji
506.The Stress Corrosion Cracking of Type 316 Stainless Steel in Oxygenated and Chlorinated High Temperature Water.[Corrosion Science,25,(1985),769-788]J. Congletton, H.C. Shih, T. shoji and R.N. Parkins
507.The Stress Corrosion Cracking of Reactor Pressure Vessel Steel in High Temperature Water..[Corrosion Science,25,(1985),633-650]J. Congleton, T. Shoji and R.N. Parkins
508.Growth Behavior of Hydraulically Created Crack and its Size Evaluation Using Well Logging Data - Crustal Rock Fracture Mechanics Approach -.[Geothermal Resources Council Trans.,9,(1985),579-584]T. Shoji, K. Hayashi, T. Kojima, T. Ito, H. Takahashi and H. Abé
509.A New In-Situ Tectonic Stress Measurements and its Application to a Geothermal Model Field.[Geothermal Resources Council Trans.,9,(1985),99-104]K. Hayashi, T. Shoji, H. Niitsuma, T. Ito and H. Abé
510.再結晶法による延性不安定破壊の評価(破壊靭性試験片と表面亀裂試験片の対比).[日本機械学会論文集(A編),51,(1985),514-517]鬼沢邦雄,庄子哲雄,高橋秀明,安藤柱
511.核融合炉大形超伝導マグネット構造材料の極低温における破壊靭性評価..[日本機械学会論文集(A編),51,(1985),2256-2264]竹内 正道,庄子 哲雄,高橋 秀明,穴山 武
512.低ひずみ速度破壊靭性試験による原子炉圧力容器鋼の環境割れ感受性の評価..[日本機械学会論文集(A編),51,(1985),714-722]安斎 英哉,庄子 哲雄,高橋 秀明,中島 甫,近藤 達男
[1984]
513.蒸気タ-ビン・発電部材の新しい非破壊的経年劣化診断技術.[電気現場技術,23(261),(1984),1-7]高橋秀明,庄子哲雄,鈴木正彦,村松正光,木村和成,斎藤潔,鈴木雅行
514.Application of Acoustic Emission to Fracture Tougness Test of Rocks under Simulated Geothermal Reservior Conditions..[PAE2,(1984),616-623]T. Shoji, K. Tamakawa, H. Takahashi and T. Wakabayashi
515.Determination of Intergranular-Cleavage Mode Fracture Toughness of Retired Steam Turbine Rotor Steel (CrMoV) by Means of Acoustic Emission Technique.[AE2,(1984),89-96]K.Shimomura, T.Shoji, H.Takahashi and K.Saito
[1983]
516.AE周波数解析によるCr-Mo-V鋼ポップイン型粒界割れの検知.[鉄と鋼,69(16),(1983),118-125]下村 慶一,庄子 哲雄,高橋 秀明
517.Characterization of Ductile Crack Growth Behaviour Based on Energy Dissipation within Intense Strain at Crack Tip..[CSNIW,(1983),428-449]T. Shoji and H. Takahashi
518.Effect of Microstructure and Strength of Low-Alloy Steels on Cyclic Crack Growth in High-Temperature Water..[ASTM Special Technical Publication 801, American Soc. for Testing and Materials,(1983),256-286]T. Shoji, H. Nakajima, H. Tsuji, H. Takahashi and T. Kondo
519.A Criterion Based on Crack-Tip Energy Dissipation in Plane-Strain Crack Growth Under Large-Scale Yielding.[ASTM STP,803,(1983),I-130-I-158]M. Saka, T. Shoji, H. Takahashi and H. Abé
520.Combined Elastic-Plastic and Acoustic Emission Methods for the Evaluation of Tearing and Cleavage Crack Extension.[ASTM STP,803,(1983),II-508-II-530]M. A. Khan, T. Shoji, H. Takahashi, and H. Niitsuma
Page: [prev] [1] [2] [3] [4] [5] [6] [7] [8] [9] [10] [11] [12] [13] [14] [15] [16] [17] [18] [19] [20] [21] [22] [23] [24] [25] [26] [27] [28] [next]
戻るこのページのトップへ
copyright(c)2005 Tohoku University